Lance, Richard,
Automobiles are exempt from RoHS, BUT there is EU ELV legislation, which
I know little about. But in another way they are not exempt - from the
effects of RoHS, because electronics suppliers to the auto industry are
going to find some parts can ONLY be procured in the Pb-free variety.
Batteries, ah now there is a can of worms. For every 100 pounds of
lead, our industry uses 1 pound (to exaggerate a bit), while the battery
boys use 80 pounds. They are quite proud of their 85% recovery rate,
which means they lose over 15X as much as we use!
And why isn't it 100%? Because, as I have stated before in this forum,
from a very interesting book called "The Economy of Waste" I read the
EPA found that primary lead smelting is done in parts of Montana and
Missouri that are not heavily populated while the secondary smelters are
all in CA, Texas and the east coast, all heavily populated. They are
concerned about airborne contamination from these smelters (so says the
book, so don't shot me!), so they have stopped pushing for 100%
recycling. The book then asks, without answering, what would happen if
we stopped all lead acid battery recyling. Now THAT statement should
elicit some response.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard
Sent: July 25, 2005 4:57 PM
To: [log in to unmask]
Subject: Re: [TN] Lead free in automotive
What is the rationale behind that? Automotive electronics are as
consumable as Sony CD players, and they all end up in a landfill, along
with the lead batteries and all of the lead solder in the wire
harnesses, etc. So how come they are exempt? One more bit of madness
with this whole lead-free thing.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Judy Brown
Sent: Monday, July 25, 2005 3:35 PM
To: [log in to unmask]
Subject: Re: [TN] Lead free in automotive
Automotive is exempt.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lance Mayes
Sent: Monday, July 25, 2005 1:21 PM
To: [log in to unmask]
Subject: [TN] Lead free in automotive
Good afternoon Technetter's;
Can anyone tell me how this "lead free fiasco" is going to affect the
automotive industry? Does this mean that all the gauges, batteries and
who knows what else is going to have to be changes over to lead free?
I'm welcoming for all comments.
Thanks in advance
P. Lance Mayes CIT
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
Mfg. Trainer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|