TechNetters,
What could be the impact of a silver contamination in a tin-lead wave
solder bath?
The silver content of the SnPb wave solder bath jumped to 0.14% (vs 0.1%
allowed) and the corresponding joints look grainy.
Can this have an impact on reliability? I seem to remind of a MIL spec
detailing the effects of different metallic contaminants but am unable
to find it.
Thanks in advance for your insights.
Best regards,
A. Grivon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------