Hi Cheryl!
IPC-600G, section 2.9.3.3 says that if a soldermask dam (web) was supposed
to be
there between a BGA and a via, it should be there, otherwise it's
nonconforming.
But it doesn't say how big the dam should be...
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
|---------+--------------------------------->
| | Cheryl Johnson |
| | <[log in to unmask]
| | ELSTOR.COM> |
| | Sent by: TechNet |
| | <[log in to unmask]> |
| | |
| | |
| | 07/21/2005 11:01 AM |
| | Please respond to |
| | TechNet E-Mail Forum |
| | <[log in to unmask]>; |
| | Please respond to |
| | Cheryl Johnson |
| | <[log in to unmask]
| | ELSTOR.COM> |
| | |
|---------+--------------------------------->
>--------------------------------------------------------------------------------------------------------------|
| |
| To: [log in to unmask]@SMTP@Exchange |
| cc: (bcc: Stephen R Gregory/LABARGE) |
| Subject: [TN] Soldermask inspection |
>--------------------------------------------------------------------------------------------------------------|
Do you know if any spec exists defining minimum soldermask webs
(particularly between vias and bga pads)?
Any inspection criteria?
Your help is appreciated.
Sincerely,
-----------------------------------
Cheryl Johnson, C.I.D.+
Manager
ExcelStor US Office, Engineering Services
Email: [log in to unmask]
Tel: (303) 684-7291
Fax: (303) 684-7268
Mobile: (303) 809-5815
-----------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|