Hi Ian:
Conformal coating under BAG is a tricky business. You have to
squirt ( not spray) first around the edges of the BAG in a special way
to avoid creating air bubbles ( no coating ) under the component. There
are products that are made for under fill of components that can be
injected after spray coating. These products will cover all the area
under a BAG and prevent dendrites growth much better than a spray
coating can. They will give the component mechanical strength.
What kind of equipment are you using to spray?
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Fox, Ian
Sent: Tuesday, July 19, 2005 12:23 PM
To: [log in to unmask]
Subject: [TN] Coating under BGA's
Fellow techies, a BGA related question. We're just starting to design
BGA's into some new designs which are class 3 high rel assemblies and I
am asking myself questions about the ability to adequately conformally
coat under the packages. Our standard coating is a solvent based acrylic
and we are using a 456PBGA device and a 429CBGA device, both on 1.27mm
pitch, as the maximum sizes so far and I'd be interested to hear what
other class 3 builders have experienced when applying the coating.
Regards
Ian Fox
Goodrich ECS
Birmingham
UK
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|