Assuming that the "no-clean" paste worked well for you.
Are the characteristics (solids content, viscosity, powder size) of the water soluble paste and the "no-clean" paste the same?
If so you should be good to go.
Jerry Dengler
Manufacturing Engineer
Pergamon Corporation
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Mauro
Sent: Friday, July 01, 2005 4:12 PM
To: [log in to unmask]
Subject: [TN] Stencil Apertures
Folks,
We are moving from a no-clean process to a clean (water soluble )process.
Some 20 mil devices. Do we need to change apertures on any devices?
Thanks in Advance
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
DLM
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|