Hi Lee,
"However a fast cool down will result in the solder joint having a smaller
grain
size. This should improve the solder joint’s fatigue resistance. I've
heard of stories where folks would "quench" with cold air the hardware
right after soldering but I never personally seen it in the shops I
supported or tried it."
That is a really bad idea. In accelerated thermal cycling, and ONLY in ACT,
will fine-grained solder structure result in an increase in creep-fatigue life
by roughly a factor of 2. The grain structure of solder will coarsen with
temperature and time following an Arrhenius relationship with an activation energy
of abour 0.52 eV, and after a year in the field--or on the shelf, you will be
unable to tell whether the initial grain structure was fine or coarse. Thus,
industry documents like IPC-9701 and IPC-SM-785 recommend accelerated aging of
test assemblies prior to ACT to start with a solder joint grain structure
equivalent to about a one-year-old solder joint. This is done to make the test
results more representative of product reliability.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|