Kemet has some great articles in this.
Where are the cracks?
Cracks in the middle are either flex cracks or problems wit the pick and
place (or some other applied force.)
Cracks at the ends are usually from thermal stress? (soldering irons)
Paul Stolar
Materials/Reliability Engineer
Manufacturing Reliability Lead Engineer
Baker Atlas
713-625-5376
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Karen Walters Ebner
Sent: Thursday, July 14, 2005 1:31 PM
To: [log in to unmask]
Subject: [TN] Cracked Passives
Would anyone list for me in most probable order the causes for cracked
capacitors. Has anyone had issues with cracked caps with SnAg Solder
paste????
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|