DESIGNERCOUNCIL Archives

July 2005

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
DesignerCouncil <[log in to unmask]>
X-To:
Designers Council Forum <[log in to unmask]>, "Allen T. Maddox" <[log in to unmask]>
Date:
Thu, 28 Jul 2005 08:19:00 -0400
Reply-To:
"(Designers Council Forum)" <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=us-ascii
Subject:
From:
Chris Ball <[log in to unmask]>
X-cc:
MIME-Version:
1.0
Parts/Attachments:
text/plain (107 lines)
I think, as always, the answer is: It depends.

If you have a run that carries 6 amps on a tiny board and you don't have
room to clear around an 0603 capacitor pad and still keep the minimum
copper width you need, or by doing so you would sacrifice another aspect of
the design, then perhaps it's OK to bury the pad in the 6A trace.

If you bury all GND pads in a plane for no particular reason, perhaps you
ought to rethink what you're doing.

I still think a big part of what we get paid for is to pick the best
compromise.

Purchasing, Packaging, Engineering, Assembly, and Test:
Pick one and imagine doing a board only from that perspective. Would that
design please the others? Or, try to imagine a design where all agreed that
what you'd done was perfect (if you can imagine that, then you're not
imagining the same kind of purchasing people I deal with - because if
suppliers were paying us for the privilege of giving us stuff, my folks
would say we should be getting paid more).

My goal is to not piss anyone off too bad. And if someone is mildly
perturbed from time to time but agrees that I did that right thing after
I've explained why, I feel pretty good.

-Chris (el CID)





                       "Allen T. Maddox"
                       <allen.t.maddox@GAI-TRONIC        To:   [log in to unmask]
                       S.COM>                            cc:
                       Sent by: DesignerCouncil          Subject:    [DC] Trace width ratio to
                       <[log in to unmask]>           pad

                       07/27/2005 02:47 PM
                       Please respond to
                       "(Designers Council
                       Forum)"; Please respond to
                       "Allen T. Maddox"







Hey Folks,

I was always told to NOT exit a pad, especially a SMT pad, with a trace the
same width of the pad for the reason of dissipating the heat off the pad
and creating soldering issues.
I have an engineer who doesn't believe me and wants proof. Does anyone have
any articles that support what I've been taught, or have I been mislead all
these years?

Thanks,


Allen Maddox C.I.D.
Sr. PC Board Designer
GAI-Tronics, Corp
610-796-5854
PO Box 1060
Reading, PA 19607-1060

[log in to unmask]
www.gai-tronics.com


*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.

This footnote also confirms that this email message has been swept
for the presence of computer viruses.

www.hubbell.com - Hubbell Incorporated

---------------------------------------------------------------------------------

DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2