Allen,
I don't have any articles to back up my statements but pads having the
same width as trace causes no soldering issues at all. If you consider
most of solder accumulates at the device side part of the pad, you'll
see there is no issue. The solder fillet forms quite nicely.
Cheers,
Ron Scott C.I.D.
Sr. PCB Designer
Texas Instruments
Storage Products Group
Tel: 214.567.4715
Cell: 972.816.7978
Fax: 972.761.5070
[log in to unmask]
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of
Allen T. Maddox
Sent: Wednesday, July 27, 2005 13:47
To: [log in to unmask]
Subject: [DC] Trace width ratio to pad
Hey Folks,
I was always told to NOT exit a pad, especially a SMT pad, with a trace
the same width of the pad for the reason of dissipating the heat off the
pad and creating soldering issues.
I have an engineer who doesn't believe me and wants proof. Does anyone
have any articles that support what I've been taught, or have I been
mislead all these years?
Thanks,
Allen Maddox C.I.D.
Sr. PC Board Designer
GAI-Tronics, Corp
610-796-5854
PO Box 1060
Reading, PA 19607-1060
[log in to unmask]
www.gai-tronics.com
*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they are
addressed. If you have received this email in error please notify the
system manager.
This footnote also confirms that this email message has been swept for
the presence of computer viruses.
www.hubbell.com - Hubbell Incorporated
------------------------------------------------------------------------
---------
DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF
DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL) Search previous postings at: www.ipc.org >
On-Line Resources & Databases > E-mail Archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|