We use stamps from VRS - the ink is red mixed with black to gain
permanence. They are self-contained stamps that can be used to mark
immediately after test since the cure is seconds. These marks will
with-stand more assembly operations but can be removed with a strong
solvent.
Take a look at: http://www.vrsmarking.com
We use Insta Mark 116.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: Fineline Circuits, Inc [mailto:[log in to unmask]]
Sent: Monday, June 27, 2005 1:25 PM
To: [log in to unmask]
Subject: [TN] Et stamps and Ink
Hi Technetters,
I would like to know what ink and stamp most board shops use to mark
boards
with ET. We used to stamp ET with a white ink but the letters ran into
each
other, they got smudged, and the ink was not permanent. Durig assembly
it
got washed out. Also the stamp pad would dry up. We need to mark boards
with ET and date code. Is there a single stamp that we could use where
you
can change the date on the stamp and the ink is permanent and the stamp
pad
doesn't dry up.
Also let know if there are other alternatives to this.
Thanks
Sona Sitapara
Fineline Circuit Inc.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|