Blair,
How old is your white board? I wonder if it is pitted? We often just
use a LITTLE IPA. But I would have expected the cleaner provided by the
marker vendor to be the best. There are stronger solvents out there,
but I hesitate to mention them, as they may take the top coat off the
board or the "top coat" off your liver (not literally obviously)!
DO NOT wax the board. Even if it did make them easier to clean, it
would be because the marker is now not touching the surface it is
supposed to and would probably look crappy, IF you could get the marker
to work. Ask the board supplier if they have some sort of rejuvenator
for their brand of board. Read the MSDS first before buying/using.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair K. Hogg
Sent: June 17, 2005 8:27 AM
To: [log in to unmask]
Subject: [TN] [NTC] - (Sort of) Need help from the chemical gurus out
there
I thought this would be a good question for Friday, not related to lead
in solder or anything similar....
We have a training / breakout room with large white boards on the walls.
The standard cleaner works OK for removing the markings left on for days
or weeks, but some still remains. Is there a better cleaning solution
(not likely, you would think that the experts in white board markers
would know how to remove this stuff if it sits dried for a while) that
will clean these boards?
Second question - can the white boards be waxed periodically to improve
their cleaning performance? What type of wax would be best?
Happy Friday,
Blair
*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.
This footnote also confirms that this email message has been swept
for the presence of computer viruses.
www.hubbell.com - Hubbell Incorporated
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|