Hi Ioan,
Well actually, the landpattern would be the size of each of the metallization
projections; about 60 mils wide and 20 mils long times two, of course.
You would inspect those solder joints the same way you inspect the solder
joints of BGAs--you do not. I always found it curious that people want to design
things so they can be better inspected, not that they function bettter.
Remember, the J-lead/gullwing arguments?
First, the CCs would swim up--the solder has nowhere to go. Second, many of
these chips are glued anyway. Third a soldermask dam underneath the CC serves
well.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|