My question is not regarding the diameter of the solder spheres after the
BGA has been placed on a board.
We reball components in order to use them in a repair environment. A solder
sphere has a different diameter once it has been reflowed onto the BGA.
I was looking for a general guideline such as if the pad is %65 of the
sphere diameter, the solder sphere will change its diameter such and such a
percentage.
David
>From: Bev Christian <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>, Bev
>Christian <[log in to unmask]>
>To: [log in to unmask]
>Subject: Re: [TN] Solder Sphere Diameter
>Date: Wed, 8 Jun 2005 17:12:38 -0400
>
>Also the weight of the part.
>Bev
>RIM
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
>Sent: June 8, 2005 5:07 PM
>To: [log in to unmask]
>Subject: Re: [TN] Solder Sphere Diameter
>
>That depends on a number of factors including the device weight vs the
>number of connections, coplanarity of the package when the solder
>solidifies
>etc.
>
>John
>------------------------------------
>Avanex
>John Burke
>Senior Manager RoHS Compliance
>[log in to unmask]
>40919 Encyclopedia Circle
>Fremont
>CA 94538
>tel: 510 897 4250
>fax: 510 979 0189
>mobile: 510 676 6312
>------------------------------------
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of David Tremmel
>Sent: Wednesday, June 08, 2005 2:00 PM
>To: [log in to unmask]
>Subject: [TN] Solder Sphere Diameter
>
>
>Technetters:
>
>If a BGA has a pad of 20 mil and a solder sphere of 30 mil, what is the
>diameter of the solder sphere after it has been soldered to the BGA?
>
>
>David
>
>_________________________________________________________________
>Visita MSN Latino Entretenimiento: ¡música, cine, chismes, TV y más...!
>http://latino.msn.com/entretenimiento/
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>
>---------------------------------------------------------------------
>This transmission (including any attachments) may contain confidential
>information, privileged material (including material protected by the
>solicitor-client or other applicable privileges), or constitute non-public
>information. Any use of this information by anyone other than the intended
>recipient is prohibited. If you have received this transmission in error,
>please immediately reply to the sender and delete this information from
>your system. Use, dissemination, distribution, or reproduction of this
>transmission by unintended recipients is not authorized and may be
>unlawful.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
_________________________________________________________________
Visita MSN Latino Noticias: Todo lo que pasa en el mundo y en tu paín, ¡en
tu idioma! http://latino.msn.com/noticias/
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|