Hi Steve,
Even that is not the whole story. In J-STD-020 & 033, MSL levels are
established. however, no differentiation is made as to the difference in the soldering
temperatures for SnPb-soldering and LF-soldering. The MSLs mean different
things depending on the soldering temperature, since at higher temperatures the
same moisture level will result in higher vapor pressures and thus more
destructive forces. Thus, some sort of de-rating system, i.e.,
MSLx(SnPb)=MSL[x+2](LF); thus, e.g., MSL3(SnPb)=MSL5(LF), needs to be developed.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|