Solder temperature and dwell time is heavily influenced by the panel design,
Leveling machine type and solder alloy used; but it will be in the range of
265-280C and 2 - 8 seconds. The thickness range will be tighter and
typically 1.5 to 12 microns. We regularly process CEM1 for customers.
If you would like us to process samples for you to determine a capability
with you panels please contact me directly..
-----Original Message-----
From: Ahmet Ferit Cožan [mailto:[log in to unmask]]
Sent: 15 June 2005 03:24 PM
To: [log in to unmask]
Subject: [TN] Lead Free HASL Process
Hi,
is there anyone that could inform me about the new lead-free HAL process
specifications. What is the new dwell time, temperature? If we want to use
CEM1 material, is there any disease probability bsecause of the thermal
shock, etc. I'll be appreciated if anyone can advice me information sources
about the new HAL procedures (Solder thickness, temperature range, dwell
time, solder bath material, etc.)
Thanks for all responses
Best regards
Ferit
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|