Ken
I think you need another supplier.
We capped vias for years on immersion silver boards in Richmond (the old AT&T facility) without these perceived problems. Capping in most cases will provided the same enhancements as plugging. It can also be carried out after the immersion silver process.
The boards we built were always in a panel format when they went through immersion silver. We were using the very first of all immersion silver processes; the processes and chemistries are now a great deal more robust and will withstand a great deal more abuse.
You may need to remind your supplier that we now live in the 21st century and they should begin the pilgrimage.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: Kanaiyalal Patel<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Friday, June 10, 2005 5:23 PM
Subject: [TN] Immersion Silver - Via Plugging
Our supplier is recommending against plugging via holes the immersion silver boards and here is their explanation. Need some input into how you guys are managing.
"We can not plug before silver because chemicals used during the silver process may become trapped. Over time these chemicals can eat away at the hole wall copper creating voids.
2. Because the boards have passed through rout and are in piece form when silver is applied the board can not be plugged in panel form as are the gold boards.
3. Immersion silver is soft and easily damaged. It is our last manufacturing process and we avoid handling it as much as possible after being coated, this particularly applies for the plug process."
Appreciate your feedback.
re,
Hemant
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|