Ho Gordon,
Just came across a paper from Celestica <
http://www.greensupplyline.com/showArticle.jhtml?articleID=164901053>, which refers to an iNEMI study, where it
was found that for every 10°C temperature increase the MSL needs to be derated
by one level.
Werner