Bill,
The SMTA in Orange County had their May meeting on this topic. You might
take a look at Kathy Palumbo's write up in the SMTA newsletter
http://www.laocsmta.org/newsletter/current.pdf on pages 3-5.
You can get more info on the STABLCOR material at www.thermalworks.com/ .
To my knowledge they've got three licensees of the process (Cirtech, DDI
and Winonics)all are Orange County board shops. You might contact them to
get an idea on what the pricing "up charge" is on using this material.
Best regards,
Scott McCurdy
IPC Designers Council - Orange County Chapter president
www.ipcdesignerscouncil.org
Western Regional Mgr.
diversifiedsystems, inc.
PC Boards and Assemblies
cell (714) 425-3235
eFax (714) 242-1952
eMail [log in to unmask]
website www.divsys.com
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of
Brooks,Bill
Sent: Wednesday, June 08, 2005 4:01 PM
To: [log in to unmask]
Subject: [DC] Stablcor substrate material
Has any of you had any experience with the STABLCOR materials for boards? I
was just reading an article in VMEbus Systems magazine about it and noticed
they are claiming that their ST600 material has almost 2 times the
conductivity of copper and the CTE is actually a little negative as
temperature rises... I'm not sure that is a good feature but the rate of
change is very small compared to FR4 and Copper. The material is also about
1/4 the density of copper so it weighs less... The only thing they don't
highlight is the cost... which speaks volumes... I would be curious to know
if anyone has used it and what their results were.
Bill Brooks - KG6VVP
PCB Design Engineer, C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
Datron World Communications, Inc. _______________________________________
San Diego Chapter of the IPC Designers Council
Communications Officer, Web Manager http://dcchapters.ipc.org/SanDiego/
http://pcbwizards.com
----------------------------------------------------------------------------
-----
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
1.8d To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF DesignerCouncil. To temporarily
stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil
NOMAIL/(MAIL) Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|