Good Morning Guenter!
Ramon Dehoyos and I have the same type of station from a
companany named CCRCO. I have a CCR2000 station. You
can visit their web page at:
http://www.ccrco.com/
We needed the station here for a customer who gave us a
contract to upgrade over 2,000 assemblies that have been
built and conformal coated with a urethane coating.
The upgrade consisted of changing components out with
ones of different values...many were through-hole components.
We didn't want to burn through the urethane (which you can do)
when changing the components, because we didn't want to take
the chance of contaminating the PTH barrel with coating.
We didn't want to use a chemical stripper to remove the coating,
because anything you use that can strip urethane can also damage
the board if you're not careful. So we decided on the CCR station.
After looking at a few different stations, we decided this was the only
one that was designed and made from the ground up to specifically
remove conformal coating from printed circuit assemblies, and do so
with the lowest possible risk from any ESD damage...this is a really
good station.
....and no, I do not have any financial interest in the company.
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
|---------+---------------------------->
| | Guenter Grossmann|
| | <Guenter.Grossman|
| | [log in to unmask]> |
| | Sent by: TechNet |
| | <[log in to unmask]>|
| | |
| | |
| | 06/07/2005 02:11 |
| | AM |
| | Please respond to|
| | TechNet E-Mail |
| | Forum; Please |
| | respond to |
| | Guenter Grossmann|
| | |
|---------+---------------------------->
>--------------------------------------------------------------------------------------------------------------|
| |
| To: [log in to unmask] |
| cc: |
| Subject: [TN] Antw: [TN] micro abrasive blasting for conformal coating removal |
>--------------------------------------------------------------------------------------------------------------|
micro shot blasting? Sounds interesting. Do you have any reference where
these things can be bought?
Best regards
Guenter
EMPA
Swiss Federal Laboratories for Materials Testing and Research
Centre for Reliability
Guenter Grossmann, Senior Engineer
8600 Duebendorf
Switzerland
Phone: xx41 1 823 4279
Fax : xx41 1 823 4054
mail: [log in to unmask]
>>> [log in to unmask] 03.06.2005 19:29:05 >>>
Has anyone used one of the micro shot blasting systems for removal of
conformal coating?
I have some concerns about static and the residue left behind. We use
a
moisture cure silicone coating, so abrasion works well to remove it,
but the
dry powder in the air stream must produce high static charges and if it
is
not possible to wash the assembly the shot residue will be left
behind.
There are multiple different shot materials offered including walnut
shell,
plastic pellet, and sodium bicarbonate. Since powders are difficult to
remove from the soft silicone coating, are there any of these materials
that
a trace residue left behind would not cause reliability issues?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|