Additional considerations are in 610D Clause 10.4.4 Flux Residues -
No-Clean Process - Appearance
Acceptable - Class 1,2,3
* Flux residue on, around, or bridging between noncommon lands,
component leads and conductors.
* Flux residue does not inhibit visual inspection.
* Flux residue does not inhibit access to test points of the assembly.
Acceptable - Class 1
Process Indicator - Class 2
Defect - Class 3
* Finger prints in no-clean residue.
Defect - Class 2,3
* Flux residue inhibits visual inspection.
* Flux residue inhibits access to test points.
Note 1. There is no defect for discoloration of OSP coated
assemblies that come in contact with flux residues from no-clean
process.
Note 2. Residue appearance may vary depending upon flux
characteristics and solder processes.
Defect - Class 1,2,3
* Wet, tacky, or excessive flux residues that may spread onto other
surfaces.
* No-clean flux residue on any electrical mating surface that inhibits
electrical connection.
Jack Crawford, IOM
IPC Director Certification and Assembly Technology
[log in to unmask]
847-597-2893
FAX 847-615-5693
3000 Lakeside Drive, Suite 309 S
Bannockburn, IL, 60015
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerry Savard
Sent: Monday, June 27, 2005 8:30 PM
To: [log in to unmask]
Subject: Re: [TN] No-clean residue requirements
IPC-A-610D, section 10.4.1, states as acceptable, Class 1,2,3 "No
discernible residue from cleanable fluxes is allowed" and "Flux residues
from no-clean processes may be allowed." The 'may be allowed' part I
believe covers the bases for those products that have to be super clean
depending on its end-usage. In general, no-clean will leave some
residue which is acceptable since it's activity is very low.
Gerry Savard
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jordan, Dave
Sent: Monday, June 27, 2005 8:46 PM
To: [log in to unmask]
Subject: [TN] No-clean residue requirements
I've got a customer claiming that the slight residue left on a board by
no-clean flux is a fault under either IPC-A-610 or J-STD-001. Perhaps
I'm missing it, but there doesn't seem to be any clear statement about
no-clean residue vs water wash in the standards. Any help out there?
Thanks in advance.
Dave
Production Operations
Nova Engineering
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|