Depending on who donates the money, studies can be fixed to benefit the donor. Most of us have read conflicting reports by prestigious organizations. Like they say, do not bite the hand that feeds you.
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Korringa, Stuart
(AGRE)
Sent: Wednesday, June 15, 2005 9:07 AM
To: [log in to unmask]
Subject: Re: [TN] Lead-Free, Why?
Yesterday I received a copy of a presentation of CALCE's Electronics
Products and Systems Center at the University of Maryland giving some
results of their lead-free solder reliability study. I was startled at
the results since I have been a lead-free basher.
My company is CALCE member and the document is confidential and
proprietary so I better not quote any of it. All I can offer is that
other interested parties contact CALCE for membership and copies of the
presentation.
Legally, I can entertain no more questions about the contents.
Gagged in Grand Rapids,
Stuart Korringa
Program Quality Engineer
Smiths Aerospace - Electronic Systems
3290 Patterson Ave. SE
Grand Rapids, MI 49512-1991
P: 616-241-8189
F: 616-241-7736
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ofer Cohen
Sent: Wednesday, June 15, 2005 9:58 AM
To: [log in to unmask]
Subject: Re: [TN] Lead-Free, Why?
Remember the Animal's farm: Two legs - bad, four legs - good?
Well, then: PB-free soldering - bad, PB-free - good...
Regards
Ofer Cohen
Manager
Quality Assurance, Reliability and Production Technologies Seabridge
Ltd. - A Siemens Company Siemens COM FN A SB
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Wednesday, June 15, 2005 2:46 PM
To: [log in to unmask]
Subject: Re: [TN] Lead-Free, Why?
Hi Phil,
Can there really be anybody left that thinks Pb-free solders are a good
thing?
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
******************************************
The information contained in, or attached to, this e-mail, may contain confidential information and is intended solely for the use of the individual or entity to whom they are addressed and may be subject to legal privilege. If you have received this e-mail in error you should notify the sender immediately by reply e-mail, delete the message from your system and notify your system manager. Please do not copy it for any purpose, or disclose its contents to any other person. The views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. The recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused, directly or indirectly, by any virus transmitted in this email.
******************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|