Hi Werner,
if I got it right, one should design the landpattern the same size as the chip? That is for a 1206, the landpattern should be 120 mils overall length and 60 mils wide.
Then, I am wondering how can one inspect the workmanship, not to mention eventual rework?
And secondly, how could one control the height of the solder joint?
Regards,
Ioan
> -----Original Message-----
> From: TechNet [SMTP:[log in to unmask]] On Behalf Of Werner Engelmaier
> Sent: Monday, June 13, 2005 5:15 PM
> To: [log in to unmask]
> Subject: Re: [TN] Ceramic MLCs and Leadfree, John Maxwell case?
>
> Hi John,
> LF-solder are stronger, less ductile, and creep slower--all of these add up
> to higher stresses in LF-SJs; ergo higher flex crack sensitivity.
> For chip components I suggest getting rid of the fillets--they cause
> component cracking, increasing the solder joint height under CCs and CRs, and reflow
> soldering them.
>
> Werner Engelmaier
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|