TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 30 Jun 2005 12:19:59 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Tempea, Ioan" <[log in to unmask]>
Parts/Attachments:
text/plain (81 lines)
Rainer,

you're right, I was confusing. The die is on an FR4 PCB, together with a few passives, this being a module. The module has to be soldered, just like any regular SMT component on a PCB.

It occurs to me more and more that this soldering on the PCB is not an issue, but the cleaning is. I will recommend encapsulation of the die prior to any subsequent handling and soldering.

Thanks,
Ioan

> -----Original Message-----
> From: TechNet [SMTP:[log in to unmask]] On Behalf Of Blomberg, Rainer (FL51)
> Sent: Thursday, June 30, 2005 12:10 PM
> To:   [log in to unmask]
> Subject:      Re: [TN] Is wire bonding reflowable?
> 
> I'm confused...isn't wire bonding actually a weld? Are we talking about IC
> leads or die wire bonds? I suppose a weld can be "re-welded" but reflow is
> not the right term.  If you mean reflow of a solder joint, that would apply
> to the leads of the IC, but wires from a die are usually not soldered,
> rather wire bonded (welded).  If the die could be protected from the
> process, reflow could be performed.
> 
> -----Rainer
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Glenn Pelkey
> Sent: Thursday, June 30, 2005 11:10 AM
> To: [log in to unmask]
> Subject: Re: [TN] Is wire bonding reflowable?
> 
> Hi Ioan,
> 
> With exposed die and wire bonds, I would say no for production.  Maybe they
> need it for a prototype...
> 
> Risk are, flux contamination, solder balls, handling damage.  The reflow
> temperature itself is not a problem, just everything that goes with it.
> 
> Glenn
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
> Sent: Thursday, June 30, 2005 7:49 AM
> To: [log in to unmask]
> Subject: [TN] Is wire bonding reflowable?
> 
> 
> Hi Technetters,
> 
> a customer of ours is wondering if a module they are ordering will be OK to
> solder in regular (SnPb for now) reflow. The module has an exposed die, no
> encapsulation, wire bonded to gold pads on an FR4 substrate. For me, since
> regular ICs can be reflowed with no issue, this module should not present
> any hickup.
> 
> My exposure to wire bonding is zero, so I take this issue with you. Can this
> question be answered as is, or would you need more details?
> 
> Thanks,
> Ioan
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2