TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0 (Apple Message framework v622)
Sender:
X-To:
Norazman Othman <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 28 Jun 2005 19:05:29 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ivanoe Pedruzzi <[log in to unmask]>
Subject:
From:
Ivanoe Pedruzzi <[log in to unmask]>
In-Reply-To:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII; format=flowed
Parts/Attachments:
text/plain (81 lines)
Hi Azman,
I used to work for hp and then for Jabil Circuit as Manufacturing
Engineer in Italy.
I changed position, but I didn't forget my background.

My suggestions are:
-start troubleshooting your process from the bottom up.
-try to see a sort of patterns in the defects you have got (board
position, frequency of the problem, date and time of happening)
-do not focus only on paste parameters, as some colleques said, it
seems the paste is fine.
-keep the viscosity consistent throughout the day (control humidity and
temperature INSIDE the screen printer)
-check for dog ears on your paste bricks. They tell you a lot on
printing process, one for all, that  there is some problem in
separating the paste from stencil.
-check for alloy presence under the stencil, right on the edge of the
apertures, if there is, then you don't have good gasketing.
-last but not least, check for complanarity parts-pcb on your pick and
place machine, component height, machine setting.
-is there only one pick&place machine? only one head to place parts? or
is there more? Do the shorts come from the same lane?
-look under a microscope how the parts sit on the paste brick, Is the
paste squeezed under the component leads? How are the leads VS the
paste bricks, centered?

- viscosity is important, metal loading in the paste is not second to
anything:  It is not the flux that withstand the weight of the parts.
-I might ask you about oven, but my experience is that it  plays
important role ONLY if everything else is under control.

Hope it will help

Ivan



Il giorno 25/giu/05, alle 11:36, Norazman Othman ha scritto:

> Thank Le Thanh Tung,
>
> Ok here are some parameters as you requested..
> Smallest fine pitch: 20mils
> Stencil design: Laser cut, 5mils of thickness, 10% reduction for fine
> pitch
> IC
> Printer: DEK288
> Solder paste: Kester EM907
>
>
> Best Regards,
> Azman
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2