No flux for electronics soldering should contain HCl or HBr. (The key word in the previous sentence is "should".)
They contain amine hydrochlorides/hydrobromides or amino acid hydrochlorides/hydrobromides, which is not at all the same thing.
(They may not be the same thing from a chemist's point of view, but if you can distinguish the difference in corrosivity AT SOLDERING TEMPERATURE between these compounds and HCl or HBr, you are much more discerning than I am...:-)
Rudy Sedlak
RD Chemical Company
---------------------------------
Yahoo! Sports
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Rekindle the Rivalries. Sign up for Fantasy Football