Hi All
Thank you for the great input. I have incorporated these possible root
causes as a set of actions for our team to go off and investigate. We are
also considering moving towards ENIG or Imm Ag as a other alternative.
Thanks again for your help!
Karen Walters Ebner
Raytheon Electronic Combat Systems
Towson, MD 21286
410.583.4082
R Sedlak <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
06/17/2005 05:05 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
R Sedlak <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] HASL Leveling
To add one more to Mr. Asbell's impressive list...
Dirty, or tarnished Copper pads prior to HAL
Rudy Sedlak
RD Chemical Company
Franklin D Asbell <[log in to unmask]> wrote:
1. Inadequate air flow
a. Low air pressure
b. block or disrupted air knives
c. dwell time (under air pressure)
d. incorrect air setting (on or off too early/late)
2. Orientation of the panel in the HASL process.
3. Temperature of the solder
4. Contaminates in the solder
Of these, cause #1 is the most likely in my experience.
Franklin
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
__________________________________________________
Do You Yahoo!?
Tired of spam? Yahoo! Mail has the best spam protection around
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
http://mail.yahoo.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|