TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 15 Jun 2005 07:51:06 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (235 lines)
Steve,
Look sending the article was NOT wasting my time. It is APPRECIATED that
you would think of us.  HOWEVER, as Dave Hillman would say, I am up to
my neck in alligators. I cannot even open the attachment right now, let
alone read it!

Apology for saying something you shouldn't have is accepted.  And since
sending the thing was not a waste of our time, apology for that is
rejected as unnecessary.

You do know how things work and you do understand that we are not
turning our industry upside down, but outside forces are - at best
misguided politicians and so-called environmentalist and at worst
self-centered politicians, economic opportunists and anarchists.

Opinions expressed are my own and do not necessarily represent those of
the company I work for, etc., etc.

Most sincerely,
Bev
RIM

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: June 15, 2005 7:42 AM
To: Bev Christian
Cc: TechNet E-Mail Forum
Subject: RE: [TN] Lead-Free, Why? NTC


Bev,

I never have considered people on this distinguished list "my personal
entertainment".
I'm sorry that you think that, and apologize sincerely if I have come
across that way.

As I said, it was the first time I have ever read that article, and I
thought that it's very
detailed and lucid about this whole lead-free thing.

Call me naive (which I probably am), I just don't understand why our
industry is being
turned upside down like this...maybe I don't know how things work.

I'm sorry I've wasted your time. Please forgive me.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX


 

                      "Bev Christian"

                      <[log in to unmask]        To:       "TechNet E-Mail
Forum" <[log in to unmask]>, <[log in to unmask]>       
                      om>                      cc:

                                               Subject:  RE: [TN]
Lead-Free, Why? NTC                                                  
                      06/15/2005 06:28

                      AM

 

 





I will be REAL blunt.  Come on. Steve.  You have been around long enough
to know how things work.  We are not here for your personal
entertainment, we have jobs to do.
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Gregory
Sent: June 14, 2005 10:17 PM
To: [log in to unmask]
Subject: Re: [TN] Lead-Free, Why?

I was kind of suprised that there was only one private response
to my post about this...I guess we all are sheep.

Let's all of us jump off the cliff, and say in the end; "We did what
we were supposed to..."

Then live with it all...

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX




                      Stephen R Gregory
                      (Tulsa)                  To:       [log in to unmask]
                                               cc:
                      06/14/2005 08:38         Subject:  [TN] Lead-Free,
Why?
                      AM





Mornin' Everyone!

Yesterday I had one of our test technicians come to me and
ask if I knew of any good reference articles about the pro's and
cons of Lead-free solders.

He's doing a assignment in his college class about manufacturing
processes. I first went on my rant about how mis-guided this whole
thing is, and then told him that I was sure I could find him some good
references.

I did a search and found one that I had never seen before, and after
reading it, I think it's the best one I've read. Go to:

http://www.cepelec.com/iso_album/leadfreehmiller.pdf

It's 53-pages, and very, very good!

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc.  It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.


__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc.  It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------




---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public
information. Any use of this information by anyone other than the
intended
recipient is prohibited. If you have received this transmission in
error,
please immediately reply to the sender and delete this information from
your system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.




__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc.  It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.







---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------