TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Dehoyos, Ramon" <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 14 Jun 2005 08:15:44 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Parts/Attachments:
text/plain (58 lines)
the dinosaurs vanished, but the small species flourished...
Ingemar

-----Original Message-----
From: Dehoyos, Ramon [mailto:[log in to unmask]]
Sent: den 13 juni 2005 15:42
To: TechNet E-Mail Forum; Ingemar Hernefjord (KC/EMW)
Subject: RE: [TN] Ceramic MLCs and Leadfree, John Maxwell case?



          The people from the countries who are forced to switch to LF solder are the ones that are going to have to pay the big price for the problems that are being caused by LF solder. The life cycle of products is going to be cut, product is going to be returned for failure to perform under warranty. Maybe it is a way for the bigger companies to get rid of the small competition.
        Ramon
	

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Friday, June 10, 2005 3:12 AM
To: [log in to unmask]
Subject: [TN] Ceramic MLCs and Leadfree, John Maxwell case?


Ave America et omnigenum.

Read a bulletin from Kemet. About MLC flex cracks and leadfree soldering.
 
Cut:
"Once the crack is created, it may not be readily detected electrically. A small DC voltage may not create sufficient stress to create a runaway state of increasing current within a short time. In the case of the flex crack, the crack can exist in a nonconductive state for a long time after creation. With time, temperature cycles, moisture exposure and increased stress levels, the crack can grow an ionic path that at first becomes noticeable leaky, then quickly deteriorates into a  highly conductive path within the ceramic dielectric. The time to failure is UNPREDICTABLE, AND CAN OCCUR IN MINUTES, HOURS, DAY, MONTHS, AND LONGER." John D. Prymak, Application Manager, Technical Marketing, July 7, 2004. Kemet USA.

The author tells that the above is now very actual because leadfree solder joints will increase the probability of flex cracks due to a harder solder. Small MCL caps are not exposed as much  as the big ones.

Personally, I thought the ductility properties of SnPb vs Leadfree were neglectable, but I may be wrong. The Kemet article rang a bell, the specialists here ran to the battle stations...
I'm too old, so I remain on my seat and just await a comfortable answer from John. Or any other proffessori ceramico...

Ingemar Hernefjord
Ericsson Microwave Systems

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2