FR-4 may with stand the wildfires
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stadem, Richard
Sent: Thursday, June 02, 2005 7:36 AM
To: [log in to unmask]
Subject: Re: [TN] FR-4 Thermal Conductivity Constant??
From what I see on the news on an almost daily basis, the material will
not have a chance to decompose from the UV in southern California. The
house will probably: 1) Slide down a hill 2)Be destroyed by wildfires
3)Be crushed in an earthquake, long before the sun has a chance to do
anything to it.
Why do they build houses on the side of a pile of wet sandstone anyway?
Doesn't take much of a lightbulb to figure out that even with high land
values, not being able to sleep at night for fear of one of the above
happening just isn't worth it.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Thursday, June 02, 2005 1:08 AM
To: [log in to unmask]
Subject: Re: [TN] FR-4 Thermal Conductivity Constant??
...and you can etch the copper so it fakes bricks or oregon pine or what
you like. Question is for how many years such a house will withstand the
UV in southern california?
Ingemar
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of John Burke
Sent: den 2 juni 2005 00:47
To: [log in to unmask]
Subject: Re: [TN] FR-4 Thermal Conductivity Constant??
Typically, from memory, it is around 0.2 Watts/Meter/degree centigrade.
In other words it would make excellent house insulation.............8-)
John Burke
------------------------------------
Avanex
John Burke
Senior Manager RoHS Compliance
[log in to unmask]
40919 Encyclopedia Circle
Fremont
CA 94538
tel: 510 897 4250
fax: 510 979 0189
mobile: 510 676 6312
------------------------------------
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of John Parsons
Sent: Wednesday, June 01, 2005 3:31 PM
To: [log in to unmask]
Subject: [TN] FR-4 Thermal Conductivity Constant??
Happy Wednesday to all,
I have a customer asking for the thermal conductivity constant for FR-4.
I have seen this spec'd on some specialty laminates, Rogers, GIL for
instance, but not on any "FR-4" laminates. Would this spec likely be
available from the laminate supplier? If not, why? Tell me why I see
it on the big $$$ high frequency laminates but not the "cheap stuff".
TIA
John Parsons
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|