TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gumpert, Ben" <[log in to unmask]>
Date:
Wed, 8 Jun 2005 15:37:47 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Taheri, Kamran" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Taheri, Kamran" <[log in to unmask]>
Parts/Attachments:
text/plain (130 lines)
Ben,
 
        Have you looked inside of your oven for little green monsters that might be doing this:)?  Have you attached TCs to both sides of these pads to verify the thermal difference?  It looks like that the pad design is reducing your placement accuracy tolerance.   




-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Gumpert, Ben
Sent: Wednesday, June 08, 2005 1:10 PM
To: [log in to unmask]
Subject: Re: [TN] mystery tombstone cause


Bev,

Yes, the direction of the tombstones on a specific board are constant
relative to that board, and are irrespective of board orientation
through the oven.

Ben

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Wednesday, June 08, 2005 8:40 AM
To: [log in to unmask]
Subject: Re: [TN] mystery tombstone cause

Ben,
When you say lift in different directions, do you mean in reference to
the board or in reference to the axis of the oven?  For instance are you
saying that on a single board you can have tombstones only facing to the
"top" of the board, irrespective of how you put I through the oven?
Hmm, is that clear?
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: June 8, 2005 8:09 AM
To: [log in to unmask]
Subject: [TN] mystery tombstone cause

Technetters,

I have several SMT board styles which give me some trouble with 0306
capacitor tombstones, and through many attempts to reduce the number of
these defects, I have found a condition that I can not seem to attribute
a cause to. I have found that across a board, all the tombstones tend to
lift in the same direction (for components in the same orientation).

I have looked at the build process, but different board styles result in
tombstones in different directions, so I believe the cause to be board
related. I have looked at solder mask registration (misregistration
occurs in various directions), power/ground plane connections by pad
(changes from location to location), and solder bumps due to HASL
(wicked pads have similar results), and nothing has led me to a root
cause.

Any ideas???

Thanks,
Ben Gumpert




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------




---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2