TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 8 Jun 2005 13:01:00 -0400
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gumpert, Ben" <[log in to unmask]>
Content-type:
text/plain; charset=iso-8859-1
Subject:
From:
"Gumpert, Ben" <[log in to unmask]>
Content-transfer-encoding:
quoted-printable
Parts/Attachments:
text/plain (58 lines)
Various component locations have different sides connected to ground or power planes. The connections to these planes are made directly by vias from the outside ends of the pads (vias are masked), so there are no traces running from the pads on either side. I have asked Stephen to post an image showing the pad configuration. This image will show a large component right next to a row of 0306 capacitors, but tombstones are in the same direction on other sides of the component, and a board run without any components except the 0306 capacitors shows the same results.

In my reflow process, I am ramping at about 1°C per second to about 165°C, slowing ramp rate (soak period) to increase another 10°C over the next minute, then ramping to peak.

Ben

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair K. Hogg
Sent: Wednesday, June 08, 2005 12:12 PM
To: [log in to unmask]
Subject: Re: [TN] mystery tombstone cause

Is one side of the component connected to a voltage or ground plane? It could be that the copper in the plane is taking heat away from the pad. One solution is to separate the pad from the plane by use of a small short trace. 

Also, if one pad has a large trace connecting to it, and one has a small trace, the large trace can also take heat away. One way to solve this is to neck down the trace right next to the pad. 

Blair

>>> [log in to unmask] 06/08/05 08:09AM >>>
Technetters,

I have several SMT board styles which give me some trouble with 0306 capacitor tombstones, and through many attempts to reduce the number of these defects, I have found a condition that I can not seem to attribute a cause to. I have found that across a board, all the tombstones tend to lift in the same direction (for components in the same orientation).

I have looked at the build process, but different board styles result in tombstones in different directions, so I believe the cause to be board related. I have looked at solder mask registration (misregistration occurs in various directions), power/ground plane connections by pad (changes from location to location), and solder bumps due to HASL (wicked pads have similar results), and nothing has led me to a root cause.

Any ideas???

Thanks,
Ben Gumpert




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

*******************************************************************
This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please notify the system manager.

This footnote also confirms that this email message has been swept for the presence of computer viruses.

www.hubbell.com - Hubbell Incorporated

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest