DSC is a test that will indicate the cure level of the material. TMA
and DMA testing may give you more information on the package integrity
over just DSC. Many labs offer this type of testing and your base
materials supplier should provide sample testing on laminate your have
purchased at no charge.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: Murulidhara [mailto:[log in to unmask]]
Sent: Wednesday, May 11, 2005 3:19 AM
To: [log in to unmask]
Subject: [TN] Tg measurement
Dear Technetters,We are manufactureing professional grade PCBs mainly
for telecommunication equipments. We do not have facilty to measure Tg
of copper clad laminates. We go by the report given by the copper clad
manufacturer.
Is it a must for PCB manufacturers to have facility for checking Tg
value. Or it is enough to go by the test report of laminate
manufacturers.
What is the method used to measure Tg. Is it very expensive. Are there
any alternate methods to check Tg.
Thanks in advance,
Regards,
Murulidhara.S
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|