TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Brooks,Bill" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Brooks,Bill
Date:
Mon, 16 May 2005 15:16:28 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (83 lines)
Barbara,

 The only 2 forms of conformal coating I have had any experience with are
Humiseal and a Acrylic Conformal coat that I cannot remember the name of...

The difference is, the Acrylic was rework-able and the Humiseal was
permanent.

Maybe someone else has more they can tell you...

Best regards,

Bill Brooks - KG6VVP
PCB Design Engineer, C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
Datron World Communications, Inc.
_______________________________________
San Diego Chapter of the IPC Designers Council
Communications Officer, Web Manager
http://dcchapters.ipc.org/SanDiego/
http://pcbwizards.com

-----Original Message-----
From: Barbara Burcham [mailto:[log in to unmask]]
Sent: Monday, May 16, 2005 2:56 PM
To: [log in to unmask]
Subject: [TN] Conformal Coating of Assembled Boards

Well, my company now has an application requiring conformal coating on
some small assembled boards. We need to mask off 3 connectors and coat
everything else.

I have some information on a product called Parylene applied by Parylene
Coating Services, Inc. in Katy, Texas.

We did a small lot with a simple spray-on process, but that is not the
way to do production runs, of course.



What would you recommend?

Thanks,

Barbara



Barbara J. Burcham, C.I.D.

Fairfield Industries, Inc

281-275-7687

[log in to unmask]




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2