That may be why the lead free initiatives supposedly don't apply to military
hardware. Now obtaining parts with SnPb terminations is another thing, the
re-ballers are going to have a field day :)
--
George Patrick
Tektronix, Inc.
Central Engineering, PCB Design Group
P.O. Box 500, M/S 39-512
Beaverton, OR 97077-0001
Phone: 503-627-5272 Fax: 503-627-5587
http://www.tektronix.com http://www.pcb-designer.com
It's my opinion, not Tektronix'
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of
Brooks,Bill
Sent: Thursday, May 26, 2005 11:08
To: [log in to unmask]
Subject: [DC] FW: [TN] USAF Airworthiness Advisory concerning Lead-Free
solders ...
This is an interesting Lead Free related development...
http://www.stevezeva.homestead.com
Look at USAFSolderAdv.PDF
Bill Brooks - KG6VVP
PCB Design Engineer, C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
Datron World Communications, Inc.
_______________________________________
San Diego Chapter of the IPC Designers Council
Communications Officer, Web Manager
http://dcchapters.ipc.org/SanDiego/
http://pcbwizards.com
-----Original Message-----
From: Stephen Gregory [mailto:[log in to unmask]]
Sent: Thursday, May 26, 2005 10:45 AM
To: [log in to unmask]
Subject: [TN] USAF Airworthiness Advisory concerning Lead-Free solders...
Hi All!
I thought that some of you may be interested in a USAF Airworthiness
Advisory (AA-05-01)concerning the use of Lead-Free solders...especially if
you're building any hardware, or doing any repair or upgrades on any USAF
Aircraft (manned or unmanned).
This Advisory hasn't been flowed-down to us yet by any of our customers. It
was dated May 9, 2005, so that may explain why it hasn't yet reached
us...but I'm sure it will. I actually got this from one of the
engineers here who got this from an associate of his that works at NORDAM
here in Tulsa.
I've posted the *.PDF on my page at: http://www.stevezeva.homestead.com
look at USAFSolderAdv.PDF. The distribution is public, so I'm not posting
anything that's privileged.
But this is another example of what a debacle this transition to
"Lead-Free" has become...
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
----------------------------------------------------------------------------
-----
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|