Yes electrolytic stress free Nickel with Hard gold should give a long and
reliable service.
If voltages/ currents are high and cost is an issue against 9999 reliability
gold is unnecessary. As the wiping action removes the nickel oxide.
Electroless nickel is hard but has phosphorus. May cause problems??
Anil Kher
micro interconnexion pvt. ltd
D3-12A, Corlim Industrial Estate
Corlim, Ilhas , Goa , India 403110
tel: 91-832-2284209/337. fax 2284209/2285271
e mail: [log in to unmask]
Leaders in Gold plated PCBs - selective/ cob
an ISO 9001-2000 Company
-----Original Message-----
From: Jeffrey Bush [mailto:[log in to unmask]]
Sent: Tuesday, May 24, 2005 1:20 AM
Subject: Re: PCB Commutator
Bright Watts NI - or a hard gold plate over low stress NI.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: Roger M Unwin [mailto:[log in to unmask]]
Sent: Monday, May 23, 2005 3:06 PM
To: [log in to unmask]
Subject: [TN] PCB Commutator
Hi Technetters,
Any suggestions for a good hard wearing finish that would extend the life of
3oz copper tracks being used as a sort of commutator. Am told that first
prototypes were made with chemical (Electroless?) gold over nickel. Some
lasted well, others not so well. Brushes are metal, sorry don't know the
composition. Approx. 5 amps current passes through connections.
Thank you for your assistance
--
Roger M Unwin
P+M Services (R) Ltd Tel : 01706 815212 Fax : 01706 818636
Http://www.p-m-services.co.uk
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|