Hi,
You say :" thermal shock 10 times and electrical test as part of screening or
burn-in."
Actually, no. The best screening procedure for SJs is vibration—most
effective and no damage to good SJs. Burn-in is not a screening procedure, just a
functional test prior to shipping.
Werner
---------------------------------------------------