We have lots of residual inventory with flux-cored solder that is many years
old. It does not have an expiration date (indefinite shelf life). The
"plastic" flux core does not seem to degrade in its inert lead sheath.
Liquid flux, on the other hand has a shelf life, but that is driven by the
volatile solvent content. Have no idea why flux-cored solder would expire
except to make you want to buy more sooner.
The flux-cored solder should be good until used up.
> Rainer G. Blomberg
> Honeywell -Space Systems Clearwater
> Staff Production Engineer
(727) 539-5534
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg A. Owens
Sent: Thursday, May 05, 2005 3:30 PM
To: [log in to unmask]
Subject: [TN] Flux Cored Solder Shelf Life
TechNetters:
A student of mine has asked, what is the shelf life of flux cored solder?
In reviewing J-STD-001 and J-STD-004 I can't find any specific guidance or
requirements from the Standards. I know newer rolls of solder (depending
upon the manufacturer) have date codes and expiration dates.
However, they have a wire solder spool still being used today that was
entered into their HazMat system in 1998 (no actual record of the precise
date of manufacture). The wire spool is removed from their HazMat system
when needed to uncontrolled/undocumented working environments within their
facility. Since the standards don't specify a shelf life, what is considered
best industry practices or is there a Standard dealing with this issue?
Thanks for your responses.
Gregg A. Owens
Master IPC Trainer
Executive Director
Manufacturing Technology Training Center, Inc.
Mira Loma, CA 91752 USA
www.mttc-inc.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|