That's when you and your wife select the same setting on your Sleep-number
bed. Sorry, due to the Holidays I missed Friday.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Roy Gregory
Sent: Tuesday, May 31, 2005 8:42 AM
To: [log in to unmask]
Subject: Re: [TN] micro cracks in leadfree wavesolder
Hi Guenter,
Would you (or someone) please explain or point me to an explanation of
"Rest-eutectic"? I (and I'm certain, others) am unfamiliar with this term.
Regards,
Ed Popielarski
QTA Machine
27291 Jardines
Mission Viejo, Ca 92692
Ph: 949-581-6601
WWW.QTA.NET
You see, wire telegraph is a kind of a very, very long cat. You pull his
tail in New York and his head is meowing in Los Angeles. Do you understand
this?
And radio operates exactly the same way: you send signals here, they receive
them there. The only difference is that there is no cat.
Albert Einstein (1879 - 1955), when asked to describe radio
********
Date: Mon, 30 May 2005 09:00:10 +0200
From: Guenter Grossmann [log in to unmask]
Subject: Antw: [TN] micro cracks in leadfree wavesolder
Ken,
No I haven't read a paper, but these microcracks are frequently seen in our
lab in failure analysis. They occur due to 3 reasons (as far as I know):
- 2 Solidification fronts meeting each other and being already too cold to
join. I believe that this is mainly a design problem.
- Shrinking of the rest- eutectic between the Sn dendrites
- Well I believe that a SnBiPb rest- eutectic is rare nowadays
Best regards
Guenter
EMPA
Swiss Federal Laboratories for Materials Testing and Research Centre for
Reliability Guenter Grossmann, Senior Engineer
8600 Duebendorf
Switzerland
Phone: xx41 1 823 4279
Fax : xx41 1 823 4054
mail: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|