Hello Technetters,
I have questions about wetting balance.
We intend to use a wetting balance not to accept/reject supplied SMD's (Our
SMD's are 1 to 5 years old) but to minimize the risk of solderability
defects in production (Low volume, SnPb technology).
So we don't apply J-STD-002D criterium but we try to find them to
corroborate wetting balance and production results.
On some tests (Wetting balance calibrated and in order, same type of flux,
same alloy) on same component lots, we have not a perfect correspondence
between wetting balance and visual inspections results in production (Vapor
phase soldering). One of the case is "Good at the solderability test/Defect
in production" and this one is the most risky.
Somebody have experience with that kind of problem?
What actions have you made ?
Thanks for answers.
Best regards,
CANTAGALLO Luigi
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|