I have XRF on order, How thick is too thick ?
-Al
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] On Behalf Of Victor G.
Hernandez
Sent: Tuesday, May 24, 2005 3:52 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Joint Anomaly
Voiding was observed in solder joint when immersion silver was very
thick.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of
[log in to unmask]
Sent: Tuesday, May 24, 2005 3:28 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Joint Anomaly
Al -
Surface finish is immersion silver? By any chance is this also a lead
free assembly?
Bruce Tostevin
Benchmark Electronics
Hudson, NH
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Al Onderick
Sent: Tuesday, May 24, 2005 3:44 PM
To: [log in to unmask]
Subject: [TN] Solder Joint Anomaly
Dear Technetters,
I now have a couple of cross sections to go along with my
xrays.
Does anyone have an idea what might cause this type of anomaly?
http://www.texas-gold.org/PCB/pages/xray/index.htm
Is this a problem or just a strange looking void ?
The board supplier is going to run the following tests
* Cross section the 15 pin connector area for optical
microscopy and analysis.
* Scanning Electron Microscopy (SEM) analysis of
solder
filled and bare silver hole wall surfaces
o SEM will identify particulate or other 3-dimensional
bodies to be analyzed with EDS.
* Energy Dispersive Spectometry (EDS) analysis of
solder filled and bare silver hole wall surfaces
o EDS will identify the all elements relative to the
point of failure to identify possible contributors as the root cause.
* X-Ray Fluorescence of bare silver hole wall
surfaces
o XRF will determine the thickness of the solder
deposit
in the hole walls in the 15 pin connector area.
-Al
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|