TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 24 May 2005 06:17:02 -0400
Reply-To:
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (35 lines)
Board separation. It is possible that the BGA is fine but the board fails
during assembly processing. This is a fairly thick board and a large I/O
BGA. I assume a fairly complex board. High aspect ratio PTH? Blind vias,
filled and plated? Food for thought.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Kerry McMullen
Sent: Monday, May 23, 2005 1:10 PM
To: [log in to unmask]
Subject: [TN] BGA Intermittents


Hi Technetters,
I have a 1089 BGA with Sn balls.
Paste is 63/37 SnPb
Board is 14 layer,  .098 thick Immersion Ag.
Ran thermocouples.  Inner balls are seeing 206 degrees C.

What could be causing intermittents at the center and corners of the BGA?

Thanks,

Kerry

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2