TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 23 May 2005 13:11:58 -0700
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Ahne Oosterhof <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
A-Laser, Inc.
MIME-Version:
1.0
Parts/Attachments:
text/plain (93 lines)
Your problem is not that uncommon (regretably). Q2 and 3 look ok, Q4 and 5
need rotation or need to be mirrored. I am not fluent in ODB++, but the same
problem shows up in Gerber. Some companies that provide viewers implement
most of the Gerber commands but forget some of the "interesting" details and
D-code or Macro rotation is one of them.

And of course there is the little detail that ODB++ is a proprietary format
belonging to Valor and they can change, extend or "improve" the format with
version changes which may or may not be compatible with previous versions,
leaving other viewer providers playing catch-up.

But once the stencil manufacturer has imported the data into their program
they should easily be able to modify the image to accommodate for this
discrepancy. Just send them a copy of the picture you get on your Valor
viewer.

Regards,
Ahne Oosterhof,
A-Laser / Fine Line Stencil, Inc.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Gregory
Sent: Wednesday, May 18, 2005 6:14
To: [log in to unmask]
Subject: [TN] ODB++ Files...

Good Mornin' all you Techno's!

Gonna be heading to San Diego this afternoon to visit a potential customer,
hope the weather is as nice as it usually is out there.

I have a question about ODB++ files. My stencil vendor called me a few days
ago after I had sent them a ODB++ file to get the stencil made for a board.
They said for some reason things didn't look right at  a few
locations...specifically at some TO 252/268 locations.

The two pads for the leads were overlaping the one big area for the base of
the footprint. I didn't have an actual board yet, so I couldn't verify the
dimensions of everything.

I have two different viewers here that are capable of viewing ODB++ files,
Autoview SolidModel by Cimmetry Systems, and a Valor Universal Viewer, of
course by Valor.

I discovered that things can look different depending on what you use to
view ODB++ files. Take a look at; "Autoview SolidModel" and Valor Universal
Viewer" on my page at; http://www.stevezeva.homestead.com

Look at the way the footprint looks for Q2, Q3, Q4, and Q5.

I just got the fab yesterday afternoon and confirmed that the image that I
see with the Valor Universal Viewer is correct. Why does different software
display ODB++ files so differently?

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver this
message to anyone.  In such event, you should destroy the message and kindly
notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2