Minimum 100 micro-inch SULFAMATE DUCTILE NICKEL PLATED
Minimum 10 micro-inch HARD GOLD PLATED
-Chris
Roger M Unwin
<[log in to unmask] To: [log in to unmask]
.UK> cc:
Sent by: TechNet Subject: [TN] PCB Commutator
<[log in to unmask]>
05/23/2005 03:05 PM
Please respond to TechNet
E-Mail Forum; Please
respond to Roger M Unwin
Hi Technetters,
Any suggestions for a good hard wearing finish that would extend the
life of 3oz copper tracks being used as a sort of commutator. Am told
that first prototypes were made with chemical (Electroless?) gold over
nickel. Some lasted well, others not so well. Brushes are metal, sorry
don't know the composition. Approx. 5 amps current passes through
connections.
Thank you for your assistance
--
Roger M Unwin
P+M Services (R) Ltd Tel : 01706 815212 Fax : 01706 818636
Http://www.p-m-services.co.uk
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
This e-mail message is intended only for the use of the intended recipient(s). The information contained therein may be confidential or privileged, and its disclosure or reproduction is strictly prohibited. If you are not the intended recipient, please return it immediately to its sender at the above address and destroy it.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|