I am assuming these are wave-solder through-hole joints? If so, my first
guess would be not enough topside pre-heat to allow the solder to flow
through, but upon further examination I realize that there is also a
large amount of voiding within the barrel, even when the solder does
flow through. Based on that, perhaps there is some type of contamination
inside the barrel. If you still have some unsoldered boards you may wish
to take a look at the cleanliness of the through-holes, and also inspect
for plating problems that could stop the solder wetting. Another
possibility is contaminated wave-solder flux, or flux with too high of
an alcohol content.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Al Onderick
Sent: Thursday, May 19, 2005 1:54 PM
To: [log in to unmask]
Subject: [TN] XRAYed through holes ??
Technetters, Any idea what might cause this? The SMT soldered fine, but
the thru holes look like this
http://www.texas-gold.org/PCB/pages/xray/index.htm
-Al Onderick
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|