ROSE testing may not be a good bet if looking specifically at the BGA area
as whatever residues underneath could end up diluted by extracting from the
whole board, and the board could pass ROSE test, though the residues in that
concentrated area could be potentially harmful and should be looked at aside
from the board as a whole.
Sara Gorcos
www.residues.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard
Sent: Thursday, May 19, 2005 9:35 AM
To: [log in to unmask]
Subject: Re: [TN] BGA test coupon
So why don't you use SIR or ROSE testing? I would think that would be
more reliable than visual inspection, as these types of flux residues
may not be easily visible, even under a glass-bodied BGA.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Charlie Pitarys
Sent: Thursday, May 19, 2005 9:29 AM
To: [log in to unmask]
Subject: [TN] BGA test coupon
Hello all, In pursuit of better cleaning I am looking for a supplier or
creative inventor that has a BGA style device/component (pick a size)
where the top is clear and you can look through and see if any flux
residue remains around the bump pattern.
My method currently employs heating up the substrate and popping off the
die,etc. The heat can skew the visual data by reheating and/or
volatilize any flux remaining etc. Plus if you have had too much coffee
during the day this exercise can get a little dicey!
I don't want to invest 30K for a spy scope either.
I know about the glass slide deal for cleaning and I am not a big fan of
it. 20+ yrs in this biz and this test method is too labor intensive and
is only designed to fail IMHO.
TIA
Charlie Pitarys
603.622.2900 x-115
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|