TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 12 May 2005 06:48:08 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Eddie Rocha <[log in to unmask]>
Subject:
From:
Eddie Rocha <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (118 lines)
95% of the ENIG bds that we build are processed thru ENIG
after LPI. This is the typical approach with ENIG bds.

As far as adhesion, there are several ways to prepare the
bare copper surface for good LPI adhesion, I.e pumice
scrub, chemical clean, microetching, etc. With the ENIG
surface you don't have all these options, but you still can
achieve acceptable adhesion.

The only valid reason to ENIG before LPI would be that if
the LPI design is covering all the vias with no reliefs.
This means there will be LPI in the holes and that can
cause problems in the ENIG process. I always want to have
all holes open to allow proper rinsing thru the ENIG
process. That's important to me.


Thank you,
Eddie Rocha
South Bay Circuits


Mornin' all you 'Netters!

Gotta question. We're getting a board quoted to buy, and
the shop has
come back for some relief on some notes on the drawing that
state:

Process Notes:

1. Plate all exposed areas with Electroless Immersion Gold
Nickel 100 microinches thk., Gold 2-10 microinches thk.
min.

2. Apply LPI soldermask over bare copper (SMOBC)
Color: Green
Conform to IPC-SM-840, Class H Current rev.
Resizing of soldermask pad clearances may be
required due to suppliers choice of material and/or
process. soldermask clearance for vias to be .004 larger
than drill hole.

The fab house is asking to plate the whole board with ENIG,
and then apply
the soldermask because they say that the ENIG process after
applying the
LPI
will make the mask look ugly.

I know the ENIG process can be tough on soldermasks, but I
thought that
problem
has already been worked out...

I gues my real question is; is the adhesion of LPI over
ENIG any worse or
better than
SMOBC?

My gut feel is to tell the fab house to comply with the
notes on the
drawing, I really
don't want to ask our customer if the fab house can deviate
from the notes
on the
drawing. But on the other hand, I don't want to get a
raggedy looking board
from
them if they don't have their ENIG processes in control...

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and
confidential to
LaBarge, Inc.  It is for use only by the individual or
entity named above.
If you are not the intended recipient, you may not copy,
use or deliver
this message to anyone.  In such event, you should destroy
the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using
LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with
following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at
[log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2