"Barmuta, Mike" <[log in to unmask]>
Date:
Thu, 12 May 2005 07:12:47 -0700
MIME-Version:
1.0
X-To:
Ted Kong <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Barmuta, Mike" <[log in to unmask]>
Parts/Attachments:
text/plain (171 lines)
Ted: We normally wipe the boards down with a clean IP impregnated wipe
cloth. This removes the majority of paste, however simply doing a wipe only
is poor practice as it leaves residues of paste behind on surface areas and
in the holes. We follow the wipe with a our standard PCA board washer which
is a conveyorized inline system using semi-aqueous chemistry (EC-Ultra), DI
rinse and dry.

                                                                Regards

Michael Barmuta

Fluke Corp.

-----Original Message-----
From: Ted Kong [mailto:[log in to unmask]]
Sent: Wednesday, May 11, 2005 5:20 PM
To: TechNet E-Mail Forum; Barmuta, Mike
Subject: Re: [TN] Washing OSP boards


Hi Mike,

Did you use IPA to clean the no-clean paste?

Ted
--- "Barmuta, Mike" <[log in to unmask]> wrote:
> Bev: It depends. :>)
> If you are using water soluble paste you should
> remove it as soon as
> possible. The higher activity level of the flux
> starts to react with the OSP
> coating.
> If you are using no-clean it's not as critical.
> However we remove(wash)the
> no-clean paste as soon as practical.
> Also it's important that the boards are thoroughly
> dried after wash. You
> don't want wet/damp boards sitting around with an
> OSP coating.
>
> We've held boards for up to a month after washing
> paste and did not
> experience any solderabilty or activation issues
> using ENTEK 106A+
>
>
>    Regards
>
>            Michael
> Barmuta
>
>            Staff
> Engineer
>
>            Fluke Corp.
>
>            Everett WA
>
>            425-446-6076
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of
> Bev Christian
> Sent: Wednesday, May 11, 2005 9:51 AM
> To: [log in to unmask]
> Subject: [TN] Washing OSP boards
>
>
> TechNetters,
> If one were to wash misprinted OSP boards would it
> be worse to
> a)  leave the solder paste on 4 hours and then wash
> and use right away
> or
> b)  wash right away and then let sit four hours
> before reprinting and
> reflowing
>
> I looked in the archives, but didn't find anything
> that was particularly
> helpful.
>
> This is a general question so I can't give solvent,
> wash time (and thus
> amount of OSP left). So, Doug P., don't give me "it
> depends" as an
> answer!
>
> Bev
> RIM
>
>
>
>
>
---------------------------------------------------------------------
> This transmission (including any attachments) may
> contain confidential
> information, privileged material (including material
> protected by the
> solicitor-client or other applicable privileges), or
> constitute non-public
> information. Any use of this information by anyone
> other than the intended
> recipient is prohibited. If you have received this
> transmission in error,
> please immediately reply to the sender and delete
> this information from your
> system. Use, dissemination, distribution, or
> reproduction of this
> transmission by unintended recipients is not
> authorized and may be unlawful.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach
> Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
>
-----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
>
-----------------------------------------------------
>

__________________________________________________
Do You Yahoo!?
Tired of spam?  Yahoo! Mail has the best spam protection around
http://mail.yahoo.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2