Edo build several designs that are close at .187 +/- 10%. I believe the
material is made by bonding 2 SS .059" cores with 8 plies of 7628. Not
cheap material but it can be done.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: Richard [mailto:[log in to unmask]]
Sent: Thursday, May 12, 2005 2:30 AM
To: [log in to unmask]
Subject: [TN] Thick PCB Fab Construction Question
Hi,
This is a question to all the fab people.
My project requires a PCB that will have a finished thickness of 4.7 mm.
I
haven't found anyone who has a standard thickness very close, but know
that
it's possible to build much thicker boards. What is the best way to
call
out such a construction?
The other significant details are:
- 2 layers, 1/2 oz. cu
- No plated through holes
- Gold flash finish, no soldermask
- Material will be in two versions, one FR4 and one in a
hi-freq.substrate
- Boards will have an additional "cover" substrate layer laminated over
the
top, but this is not included in the 4.7 mm thickness
I hope that was clear enough.
Thank you very much for any light you can shed on this.
Richard
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|