Murulidhara,
I think you would generally trust the data coming from your laminant
supplier. If you had a failure that appeared to be the material you could
ask them to retest retains or from your stock. If you had doubts at that
point you could use an independent lab with a DSC or a TAM, both fairly
expensive piece of equipment that require a level of expertise to operate.
Make sure you compare the Tg to the UTg and the difference should only be
about 2 or 3 C.
Chuck Brummer
-----Original Message-----
From: Murulidhara [mailto:[log in to unmask]]
Sent: Wednesday, May 11, 2005 12:19 AM
To: [log in to unmask]
Subject: [TN] Tg measurement
Dear Technetters,We are manufactureing professional grade PCBs mainly for
telecommunication equipments. We do not have facilty to measure Tg of copper
clad laminates. We go by the report given by the copper clad manufacturer.
Is it a must for PCB manufacturers to have facility for checking Tg value.
Or it is enough to go by the test report of laminate manufacturers.
What is the method used to measure Tg. Is it very expensive. Are there any
alternate methods to check Tg.
Thanks in advance,
Regards,
Murulidhara.S
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|