TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Alcorn, Brent" <[log in to unmask]>
Date:
Wed, 11 May 2005 10:03:31 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jenny Prosmitsky <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Jenny Prosmitsky <[log in to unmask]>
Parts/Attachments:
text/plain (243 lines)
 

yes it usually is 80%, though when the ball gets to .60mm diameter +
it's 75%

 

------------------------------

 

If you're interested I have some routing guidelines for BGA's of 1mm,
.8mm,  and  .5mm pitches.

 

On 10 May 2005 at 11:59, John Guy wrote:

 

Hello All,

        I was wondering if there is some guideline for the recommended
pad size for a BGA based on the component's ball size?  I have been told
that it is recommended that the pad diameter be about 80% of the ball
diameter, but I would like some confirmation.

 

Thanks in advance,

John Guy

Surface Mount Process Engineer

diversifiedsystems, inc

-------------------------------------

Depends if you want to have solder mask defined pads or not.

If mask defined then a rule of thumb is to aim for the same mask
aperture on the interposer. Non mask defined ROT is to make the pad
equal the minimum ball diameter so that solder joint forms around the
pad sides improving stress resistance. Although, watch out for ball
collapse, and consider what height is left if your needing to clean
after reflow, and if there is enough annulus for via in pad (if your
forced down the HDI route).

 

Generally, the larger higher value device manufacturers will give some
guidance. Altera and Xilinx have apps notes, some stuff at Intel and IBM
as well if you've got time to search. If your using an EMS then they
probably have their own preferences, best to go along with them because
it's their job to stick the bits down on the board with electric glue.

 

Some apps notes: http://www.asat.com/products/library/fg1033.pdf

http://www.altera.com/literature/an/an114.pdf

 

The National Physical Lab in the UK also a wealth of data
http://www.npl.co.uk/ on solder joint reliability including Pb free.

 

Here's a thought: With all this political correctness stuff prevailing
(no naughty words etc), how do you folks on the sunny side of the
Atlantic get away with saying 'solder' and 'soldering' all of the time?

 

Best Regards

 

David Greig

 

 

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Alcorn, Brent
Sent: Tuesday, May 10, 2005 12:09 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Ball/Pad Size Ratio

 

Hi John,

 

That is correct, see IPC SM-782 rev A amendment 2, section 14.

 

Brent

 

 

 

-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of John Guy

Sent: Tuesday, May 10, 2005 12:59 PM

To: [log in to unmask]

Subject: [TN] BGA Ball/Pad Size Ratio

 

Hello All,

        I was wondering if there is some guideline for the recommended

pad size for a BGA based on the component's ball size?  I have been told

that it is recommended that the pad diameter be about 80% of the ball

diameter, but I would like some confirmation.

 

Thanks in advance,

John Guy

Surface Mount Process Engineer

diversifiedsystems, inc.

 

Custom Products Division

3939 W. 56th Street

Indianapolis, IN 46254-4961

 

Telephone: 317-299-9547, x336

Fax: 317-298-2055

E-mail: [log in to unmask]

Web: www.divsys.com

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------

 

****************************************************************

The information transmitted in this message is confidential and may be
privileged.  Any review, retransmission, dissemination, or other use of
this information by persons or entities other than the intended
recipient is prohibited.  If you are not the intended recipient, please
notify Analogic Corporation immediately - by replying to this message or
by sending an email to [log in to unmask] - and destroy all
copies of this information, including any attachments, without reading
or disclosing them.

 

Thank you.

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text
in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:
http://listserv.ipc.org/archives

Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815

-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2